Emulsified Asphalt
NO. | Test Items | Standard No. Of Test Method | Type |
1 | Evaporation Residue | JTJ 052/T 0651 | |
2 | Residue On Sieve | JTJ 052/T 0652 | |
3 | Particle Charge | JTJ 052/T 0653 | TR-TC-0653 Emulsified Asphalt Particle Charge Tester |
4 | Mineral Aggregate Adhesion | JTJ 052/T 0654 | |
5 | Bin Stability | JTJ 052/T 0655 | TR-TC-0655 Emulsified asphalt storage stability tester |
6 | Low Temperature Storage Stability | JTJ 052/T 0656 | |
7 | Cement Mixing Test | JTJ 052/T 0657 | |
8 | Demulsification Speed | JTJ 052/T 0658 | |
9 | Mixing Test With Mineral Material | JTJ 052/T 0659 | |
10 | Low-temperature Properties Of Asphalt and Stone | JTJ 052/T 0660 | |
11 | Consistency | JTJ 052/T 0751 | TR-TC-0751 Emulsified asphalt consistency tester |
12 | Wet Wheel Abrasion | JTJ 052/T 0752 | TR-TC-0752 Wet wheel abrasion tester |
13 | Initial Setting Time | JTJ 052/T 0753 | |
14 | Adhesive Force | JTJ 052/T 0754 | TR-TC-0754 Cohesion tester |
15 | Load Wheel Rolling | JTJ 052/T 0755 | TR-TC-0755 Load wheel rolling tester |
16 | Distillation Residue | SH/T 0099.16 SH/T 0099.17 |